1.0323 (USD7)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Steels with Average C < 0,12% or Rm < 400 MPa |
Chemical composition
| Standard |
Fe, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
N, % |
| DIN 17145 |
98.783–99.49 |
0.45–0.65 |
< 0.12 |
< 0.17 |
< 0.12 |
< 0.025 |
0.06–0.1 |
< 0.025 |
< 0.007 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 7,87 g / cm³ |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| N |
% |
Nitrogen |