1.4116 (X50CrMoV1)
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Stainless Steel with Ni < 2.5% and Mo but without Nb and Ti |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| EN 10088-1 |
81.395–84.95 |
< 1 |
< 1 |
14–15 |
0.1–0.2 |
< 0.04 |
0.45–0.55 |
< 0.015 |
0.5–0.8 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
|
|
|
|
annealing, soft |
850–900 |
12 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
|
annealing, soft |
280 |
Analogues
| CIS, Russia, Ukraine |
| ZI128 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |