ZI128 (50X14MF)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-3909-85 |
81.415–87.03 |
< 1 |
< 1 |
12–15 |
0.1–0.15 |
< 0.045 |
0.42–0.56 |
< 0.03 |
0.45–0.8 |
Information on suppliers
Properties
| Property |
| Typical Characteristics Annealing Hardness HB: <255 |
| Tempering with tempering Hardness HRC: <55 |
| Calculated Properties Density: 7.72 g / cm3 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |