1.4767 (CrAl205)
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Heat Resistant Steels with Ni < 2.5% |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Al, % |
P, % |
C, % |
S, % |
|
69.825–76.5 |
< 1 |
< 1 |
19–22 |
4.5–6 |
< 0.045 |
< 0.1 |
< 0.03 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
|
13 |
7200 |
0.46 |
1.37 |
| 100 |
|
|
|
|
1.37 |
| 200 |
|
|
|
|
1.38 |
| 300 |
|
|
|
|
1.38 |
| 400 |
12 |
|
|
|
1.39 |
| 500 |
|
|
|
|
1.41 |
| 600 |
|
|
|
|
1.42 |
| 700 |
|
|
|
|
1.43 |
| 800 |
14 |
|
|
|
1.44 |
| 900 |
|
|
|
|
1.44 |
| 1000 |
15 |
|
|
|
1.45 |
| 1100 |
|
|
|
|
1.45 |
| 1200 |
|
|
|
|
1.45 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
|
|
|
|
|
< 600 |
|
|
|
|
0.02–0.63 |
|
|
|
< 6 |
|
|
|
0.63–0.125 |
|
|
|
< 8 |
|
|
|
0.125–0.5 |
|
|
|
< 10 |
|
|
|
0.5–1 |
|
|
|
< 10 |
|
|
|
> 1 |
|
|
|
< 12 |
|
Analogues
| CIS, Russia, Ukraine |
| EI595 |
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$c\cdot 10^{-3}$$ |
$$\frac{J}{kg\cdot K}$$ |
The specific heat of the material (range 20°C–T) |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |