01H25T-VI (CHS75-VI)
Steel 01H25T-VI (obtained by vacuum-induction melting) is used in various fields: oil, engineering, construction, and also in the food industry. Sheets, strips, pipes and connecting parts are made from it. Wire 01H25T-VI is also used for welding.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-3547-83 | 71.85–75.85 | < 0.5 | < 0.7 | 24–26 | 0.15–0.35 | < 0.15 | < 0.4 | < 0.015 | < 0.01 | < 0.015 | < 0.01 |
Information on suppliers
Physical characteristics
| Temperature, °C | Cp, Дж/кг·К |
|---|---|
| 100 | 460 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Alloy | TU 14-1-3547-83 | 430 | 220 | 22 |
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 | |
| TU 14-1-3547-83 | TU 14-1-3547-83 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| Cp | Дж/кг·К | Specific heat of material |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |