03H18N11
Resistant to organic and fruit acids devices and parts in the production of food, soap, oils and artificial fibers. Equipment resistant to 70% nitric, adipic acid, ammonium nitrate up to 300 degrees. OZL-22 electrodes
products working in the nitric acid medium at an elevated temperature; austenitic steel
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant ordinary steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | 65.615–72.5 | < 0.8 | < 2 | 17–19 | 10.5–12.5 | < 0.035 | < 0.03 | < 0.02 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | $$\psi$$, % | Treatment |
|---|---|---|---|---|---|---|---|---|---|
| Rod | GOST 5949-75 | < 60 | 440 | 155 | 40 | 55 | Hardening of 1020-1100 ° C, air cooling | ||
| Forgings | GOST 25054-81 | 441 | 176 | 40 | 45–55 | ||||
| The plates | GOST 7350-77 | 490 | 196 | 40 | hardening | ||||
| Sheet | GOST 5582-75 | 490 | 196 | 40 | Hardening of 1050-1080 ° C, cooling water |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Forgings | GOST 25054-81 | 1790 |
Analogues
| USA | Germany |
|---|---|
| S30403 | 1.4306 (X2CrNi19-11) |
Standards
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$\psi$$ | % | Reduction in cross section on fracture |