03Х24Н6АМ3Л (EI130)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
C, % |
Mo, % |
N, % |
| TU 00218325-20-2000 |
60.73–67.4 |
< 0.1 |
< 1.5 |
24–26 |
6–8 |
< 0.03 |
2.5–3.5 |
0.1–0.14 |
Information on suppliers
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| C |
% |
Carbon |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |