05H18N10T (0X18X10T)
for manufacturing bellows expansion joints,
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant high alloy steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | 66.495–73 | < 0.8 | 1–2 | 17–18.5 | < 0.6 | < 0.3 | 9–10.5 | < 0.2 | < 0.035 | < 0.05 | < 0.02 | < 0.3 | < 0.2 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| X 6 CrNiTi 18-10 S | Stainless Type 321 |
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 |