for details, heat-resistant up to 750 degrees. FROM; resistant to intergranular corrosion
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Steels and alloys for castings | Steel for casting with special properties |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 977-88 | 65.565–73.8 | 0.2–1 | 1–2 | 17–20 | < 0.3 | 8–11 | < 0.035 | < 0.07 | < 0.03 |
Information on suppliers
Mechanical properties at 20 °C
Analogues
| USA | Germany |
|---|---|
| J92730 | 1.4308 (GX5CrNi19-10) |
Standards
| Standard | Description |
|---|---|
| GOST 977-88 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$\psi$$ | % | Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |