Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | 73.412–77.85 | < 0.8 | < 0.003 | < 0.8 | 16.5–18 | 0.15–0.35 | 5.5–6.5 | < 0.035 | < 0.08 | < 0.02 |