09H16N15M3B (EI847, X16H15M3V)
superheater tubes and high pressure steam lines, continuously operating at temperatures up to 350 ° C.; austenitic steel
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant high alloy steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | 61.355–67.9 | < 0.8 | < 0.8 | 15–17 | 14–16 | < 0.035 | < 0.09 | < 0.02 | 0.6–0.9 | 2.5–3 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| 1.4583 | 318 |
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 |