15H18N12S4TYU (EP502, EI793, EI654)
Welded products operating in air and corrosive environments.
welded constructions, working in air and aggressive environments; steel austenitic — ferritic class
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant ordinary steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | 61.215–67.05 | 3.8–4.5 | 0.5–1 | 17–19 | 0.4–0.7 | 11–13 | 0.13–0.35 | < 0.035 | 0.12–0.17 | < 0.03 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | $$\psi$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | Treatment |
|---|---|---|---|---|---|---|---|---|---|---|
| Rod | GOST 5949-75 | 60 | 720 | 375 | 25 | 40 | 780 | Hardening of 950-1050 ° C, cooling water | ||
| Forgings | GOST 25054-81 | < 600 | Longitudinal | 715 | 382 | |||||
| The plates | GOST 7350-77 | 690–930 | 345 | 30 | Hardening of 1020-1050 ° C, cooling water | |||||
| Sheet | GOST 5582-75 | 720 | 345 | 30 | Hardening of 1020-1050 ° C, the water | |||||
| The sheet is thin and hardened. | GOST 5582-75 | 880 | 685 | 10 | ||||||
| Sheet | GOST 4986-79 | 690 | 13–25 | Hardening of 1020-1050 ° C, cooling water | ||||||
| The sheet is thin and hardened. | GOST 4986-79 | 830–1080 | 5–10 |
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 | |
| TU 14-1-561-73 | |
| TU 14-1-915-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$\psi$$ | % | Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |