Chemical composition
| Standard |
Fe, % |
Mn, % |
Cr, % |
C, % |
| GOST 5632-72 |
77.6–81.7 |
9–11 |
9–11 |
0.3–0.4 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Alloy |
|
|
|
|
700 |
400 |
16 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| C |
% |
Carbon |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |