45H22N4M3 (EP48, 4Х22Н4М3)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Heat resistant steels and alloys |
Heat resistant high alloy steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| GOST 5632-72 |
66.185–71.15 |
0.1–1 |
0.85–1.25 |
21–23 |
4–5 |
< 0.035 |
0.4–0.5 |
< 0.03 |
2.5–3 |