4H5MFS (4H5MF1S, 4H4VMFS)
For small dies, tools for horizontal forging machines.
small hammer dies, large (cross-section of more than 200 mm) and the Molotov-press inserts the hot deformation of structural steel and non-ferrous alloys in large-scale and mass production, mold injection molding of aluminum and zinc, and magnesium alloys.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tool steel |
Die tool steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| GOST 5950-2000 |
89.64–92.58 |
0.9–1.2 |
0.2–0.5 |
4.5–5.5 |
< 0.3 |
< 0.4 |
0.3–0.5 |
< 0.03 |
0.32–0.4 |
< 0.03 |
1.2–1.5 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
29 |
7750 |
0.48 |
| 100 |
30 |
7724 |
|
| 200 |
30 |
7697 |
|
| 300 |
31 |
7670 |
|
| 400 |
33 |
7641 |
|
| 500 |
31 |
7600 |
|
| 600 |
30 |
7573 |
|
| 700 |
28 |
7546 |
|
| 800 |
26 |
7520 |
|
| 900 |
27 |
7495 |
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Metal rolling |
|
10 |
|
|
1750 |
1480 |
570 |
Hardening of 1000-1020 ° C, and Holidays 530-560 ° C, 500-520 ° C and Holidays |
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
GOST 5950-73 |
annealing |
241 |
Critical point temperatures
| Ac1, K |
Ac3(Acm), K |
Ar3(Arcm), K |
Ar1, K |
Mn, K |
| 840 |
870 |
810 |
735 |
300 |
Analogues
| USA |
Germany |
Japan |
France |
United Kingdom |
European Union |
Italy |
Spain |
China |
Bulgaria |
Poland |
Romania |
Czech Republic |
Austria |
| H11 |
1.2343 (X38CrMoV5-1) |
SKD6 |
X37CrMoV51KU |
2343 |
X37CrMoV5-1 |
UD12 |
X37CrMoV5 |
4Cr5MoSiV |
X37CrMoV5-1 |
WCL |
39VSiMoCr52 |
19552 |
BOHLERW300 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |
Description of temperatures of critical points
| Parameter |
Units of measurement |
Description |
| Ac1 |
K |
|
| Ac3(Acm) |
K |
|
| Ar3(Arcm) |
K |
|
| Ar1 |
K |
|
| Mn |
K |
|