GOST 5950-2000
Information about the standard
| Standard | GOST 5950-2000 |
|---|---|
| Country | CIS, Russia, Ukraine |
| Type of standard | ГОСТ |
| Description | GOST |
| Materials | 11H4V2MF3S2, 11HF, 12x1, 13X, 3H2MNF, 3H3M3F, 4H2V5MF, 4H3VMF, 4H4VMFS, 4H5MF1S, 4H5MFS, 4H5V2FS, 4HMFS, 4HMNFS, 4HS, 5H2MNF, 5H3V3MFS, 5HNM, 5HNV, 5HNVS, 5HV2SF, 6H3MFS, 6H4M2FS, 6H6V3MFS, 6HS, 6HV2S, 6HVG, 7H3, 7HG2VMF, 8H4V2MFS2, 8H6NFT, 8HF, 8x3, 9G2F, 9H1, 9H5VF, 9HF, 9HFM, 9HVG, 9XC, CHC, CVH, DI22, DI23, DI32, DI37, DI55, DI80, EI-2, H12F1, H12VMF, H6VF, HVSGF, Tool alloy steel 250X25V3TL, V2F, X12 |