4H5V2FS (EI958, 40H5V2FS)
Another designation EI958. Temperature of critical points: Ac1 = 800, Ac3 (Acm) = 875, Ar3 (Arcm) = 840, Ar1 = 730, Mn = 275. Hardness after annealing (GOST 5950−2000): HB 10 -1 = 241 MPa .
mold die casting of zinc, aluminum and magnesium alloys, Molotov and pressing the insert (section 200−250 mm) at the hot deformation of structural steels, tool for landing pieces of alloy structural and heat-resistant materials on horizontal forging machines.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tool steel |
Die tool steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
W, % |
| GOST 5950-2000 |
88.54–92 |
0.8–1.2 |
0.15–0.45 |
4.5–5.5 |
< 0.3 |
< 0.4 |
0.6–0.9 |
< 0.03 |
0.35–0.45 |
< 0.03 |
1.6–2.2 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Metal rolling |
|
10 |
|
|
1760 |
1690 |
300 |
Hardening of 1030-1050 ° C, the oil, leave 560-580 ° C, 530-540 ° C and Holidays |
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
GOST 5950-73 |
annealing |
241 |
Critical point temperatures
| Ac1, K |
Ac3(Acm), K |
Ar3(Arcm), K |
Ar1, K |
Mn, K |
| 800 |
875 |
840 |
730 |
275 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| W |
% |
Tungsten |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |
Description of temperatures of critical points
| Parameter |
Units of measurement |
Description |
| Ac1 |
K |
|
| Ac3(Acm) |
K |
|
| Ar3(Arcm) |
K |
|
| Ar1 |
K |
|
| Mn |
K |
|