4HMFS (40HSMF)
The temperature of critical points Ac 1 = 760, Ac 3 (Ac m) = 805, Ar 3 (Arc m) = 710, Ar 1 = 630, Mn = 280. Hardness after heat treatment (GOST 5950−2000): HB 10 -1 = 241 MPa.
steam-hammer dies and pneumatic hammers with falling parts weighing up to 3 tons with deformation of structural alloyed and stainless steels, pressing tools for the machining of aluminum alloys, inserts and punches landing on horizontal forging machines.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tool steel |
Die tool steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| GOST 5950-2000 |
93.69–95.93 |
0.5–0.8 |
0.5–0.8 |
1.5–1.8 |
< 0.3 |
< 0.4 |
0.3–0.5 |
< 0.03 |
0.37–0.45 |
< 0.03 |
0.9–1.2 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\psi$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Stamping |
|
< 500 |
|
|
1450 |
1280 |
7 |
20 |
200 |
Tempering 950 ° C, oil, leave 550 ° C |
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
GOST 5950-73 |
heat-treated |
241 |
Critical point temperatures
| Ac1, K |
Ac3(Acm), K |
Ar3(Arcm), K |
Ar1, K |
Mn, K |
| 760 |
805 |
710 |
630 |
280 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\psi$$ |
% |
Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |
Description of temperatures of critical points
| Parameter |
Units of measurement |
Description |
| Ac1 |
K |
|
| Ac3(Acm) |
K |
|
| Ar3(Arcm) |
K |
|
| Ar1 |
K |
|
| Mn |
K |
|