5HNV
For molotovy stamps of steam-air and pneumatic hammers.
for steam-hammer dies and pneumatic hammers with falling parts weighing up to 3 tons
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tool steel |
Alloy tool steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
W, % |
| GOST 5950-2000 |
94.54–96.6 |
0.1–0.4 |
0.5–0.8 |
0.5–0.8 |
< 0.3 |
1.4–1.8 |
< 0.03 |
0.5–0.6 |
< 0.03 |
0.4–0.7 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\psi$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Alloy |
|
|
|
|
1280 |
1050 |
11 |
45 |
400 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
GOST 5950-73 |
annealing |
255 |
Critical point temperatures
| Ac1, K |
Ac3(Acm), K |
Mn, K |
| 730 |
780 |
205 |
Analogues
| Germany |
USA |
Japan |
France |
United Kingdom |
European Union |
Italy |
Poland |
Czech Republic |
Austria |
| 1.2714 |
L6 |
SKT4 |
55NCDV7 |
BH224/5 |
55NiCrMoV7 |
56NiCrMoV7KU |
WNLV |
19663 |
W501 |
| 55NiCrMoV6 |
|
|
|
|
|
|
|
|
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| W |
% |
Tungsten |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\psi$$ |
% |
Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |
Description of temperatures of critical points
| Parameter |
Units of measurement |
Description |
| Ac1 |
K |
|
| Ac3(Acm) |
K |
|
| Mn |
K |
|