9HF (90HF)
For frame, band, circular planers, cold work stamps, knives, edging
dies, punches, center pins.
for the frame, tape, circular saws planer; stamps for cold work; knives for cold metal cutting, cutting dies and puasonov in cold cutting burr; center punches
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tool steel | Alloy tool steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5950-2000 | 96.34–98.25 | 0.1–0.4 | 0.3–0.6 | 0.4–0.7 | < 0.3 | < 0.4 | 0.15–0.3 | < 0.03 | 0.8–0.9 | < 0.03 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Alloy | GOST 5950-73 | heat-treated | 241 |
Critical point temperatures
| Ac1, K | Mn, K |
|---|---|
| 700 | 215 |
Analogues
| USA | Germany | Japan | Bulgaria | Poland | Czech Republic | Austria |
|---|---|---|---|---|---|---|
| L2 | 1.2056 (90Cr3) | SKC11 | 8ChF | NCV1 | 19419 | BOHLERB400 |
| 1.1056 | ||||||
| 80CrV2 |
Standards
| Standard | Description |
|---|---|
| GOST 5950-2000 | GOST |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
Description of temperatures of critical points
| Parameter | Units of measurement | Description |
|---|---|---|
| Ac1 | K | |
| Mn | K |