9HFM
circular saws and wood frame
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tool steel |
Alloy tool steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| GOST 5950-2000 |
96.09–98.1 |
0.1–0.4 |
0.3–0.6 |
0.4–0.7 |
< 0.3 |
< 0.4 |
< 0.03 |
0.8–0.9 |
< 0.03 |
0.15–0.25 |
0.15–0.3 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
Treatment |
| Tape |
|
0.1–4 |
|
annealing |
930 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |