ADM
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
Примеси, % |
OE, % |
| GOST 21631-76 |
< 0.1 |
< 0.15 |
< 0.1 |
< 0.1 |
> 99 |
< 0.15 |
< 0.05 |
Information on suppliers
Analogues
| Germany |
European Union |
USA |
| 3.0185 |
P-Al99.0 |
1200 AA |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| OE |
% |
Other items |
| Примеси |
% |
Impurities |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |