AK12ch aluminum alloy (SIL-1)
Chemical composition
| Fe | Si | Mn | Ti | Al | Cu | Ca | Zn |
| up to 0.5 | 10 — 13 | up to 0.4 | up to 0.13 | 85.81 — 90 | until 0.02 | until 0.08 | until 0.06 |
Silumin in pigs is used in mechanical engineering and for the manufacture of food products. Technical requirements — according to: GOST 1583−93 Cast aluminum alloys. Technical conditions GOST R 55375−12 Primary aluminum and alloys based on it. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Ca, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.5 | 10–13 | < 0.08 | < 0.4 | < 0.13 | < 0.02 | < 0.06 | 85.81–90 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| GK-AlSi12 | BAlSi-4 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ca | % | Calcium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |