Alloy aluminum AK12M2 (AK11M2)
Chemical composition
| Fe | Si | Mn | Ni | Ti | Al | Cu | Pb | Mg | Zn | Sn | Impurities |
| 0.6 — 1 | 11 — 13 | up to 0.5 | up to 0.3 | up to 0.2 | 81.55 — 86.6 | 1.8 — 2.5 | up to 0.15 | up to 0.2 | up to 0.8 | up to 0.1 | total 2.2 |
For the manufacture of ingots and shaped castings by injection molding. Technical requirements according to GOST 1583−93
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | 0.6–1 | 11–13 | < 0.1 | < 0.2 | < 0.5 | < 0.2 | 1.8–2.5 | < 0.8 | < 0.3 | 81.25–86.6 | < 0.15 |
Information on suppliers
Brinell hardness number
Analogues
| Germany | USA |
|---|---|
| EN AB-46100 | SG 102A |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |