Aluminum alloy AK12P
Chemical composition
| Fe | Si | Mn | Ti | Al | Cu | As | Zr | Pb | Be | Mg | Zn | Impurities |
| up to 1.5 | 10 — 13 | 0.01 — 0.5 | up to 0.1 | 83.64 — 89.99 | up to 0.6 | up to 0.015 | up to 0.1 | up to 0.15 | up to 0.0005 | up to 0.1 | up to 0.3 | total 2.7 |
For the manufacture of food products. Technical requirements in accordance with GOST 1583−93
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % | Pb, % | As, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 1.5 | 10–13 | < 0.0005 | < 0.1 | 0.01–0.5 | < 0.1 | < 0.6 | < 0.3 | < 0.1 | 83.6345–89.99 | < 0.15 | < 0.015 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |