Aluminum Alloy AK13
Chemical composition
| Fe | Si | Ti | Al | Cu | Mg | Zn | Impurities |
| up to 1.1 | 11 — 13.5 | up to 0.2 | 84.9 — 88.9 | up to 0.1 | 0.1 — 0.2 | up to 0.15 | total 1.55 |
For the manufacture of ingots and castings by various casting methods (in sand molds, by investment casting, in chill molds, injection molding. Technical requirements — in accordance with GOST 1583−93 Cast aluminum alloys. Specifications. GOST R 55375−12 Primary aluminum and alloys on it. basis.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 1.1 | 11–13.5 | 0.1–0.2 | < 0.2 | < 0.1 | < 0.15 | 84.75–88.9 |
Information on suppliers
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |