AK5M2P
For the manufacture of food products.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | As, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 1.3 | 4–6 | < 0.0005 | 0.2–0.8 | 0.2–0.8 | 0.05–0.2 | 1.5–3.5 | < 0.3 | < 0.5 | 86.4345–94.05 | < 0.15 | < 0.015 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |