Alloy aluminum AK5M4 (AL5)
Chemical composition
| Fe | Si | Mn | Ni | Ti | Al | Cu | Mg | Zn | Impurities |
| up to 1.4 | 3.5 — 6 | 0.2 — 0.6 | up to 0.5 | 0.05 — 0.2 | 84.8 — 93.05 | 3 — 5 | 0.2 — 0.5 | up to 1.5 | total 3.2 |
| Note: In pigs, the magnesium content is 0.25 — 0.55% |
For the manufacture of ingots and shaped castings by various casting methods (in sand molds, lost wax, chill molds, injection molding) Technical requirements GOST 1583−93 Cast aluminum alloys. Technical conditions GOST 1583−93 Cast aluminum alloys. Technical conditions GOST R 55375−12 Primary aluminum and alloys based on it. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 1.4 | 3.5–6 | 0.2–0.5 | 0.2–0.6 | 0.05–0.2 | 3–5 | < 1.5 | < 0.5 | 84.3–93.05 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 1583-93 | in chill mold | 118–196 |
Brinell hardness number
Analogues
| USA | Germany |
|---|---|
| A03080 | G-AlSiCu4 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |