Aluminum alloy AK5Mch
- Chemical composition:
| Al | Aluminum | Rest |
| B | Boron | <0.1 |
| Fe | Iron | <0.3 |
| Si | Silicon | 4.5 — 5.5 |
| Mg | Magnesium | 0.45 — 0.60 |
| Mn | Manganese | <0.1 |
| Cu | Copper | 1.0 — 1.5 |
| Sn | Tin | <0.01 |
| Ti | Titanium | 0.08 — 0.15 |
| Zn | Zinc | <0.3 |
| Zr | Zirconium | <0.15 |
| Ot | Total impurities | <0.6 |
Casting methods:
Z — sand casting
B — Lost wax casting
K — chill casting
D — injection molding
Mark designation:
h — clean
bees — high purity
och — high purity
l — casting alloys
c — selective
Analogs in Germany
EN AB-45300 DIN EN 1676: 2010
EN AB-AlSi5Cu1Mg DIN EN 1676: 2010
EN AB-45300 DIN EN 1676: 2019
EN AB-AlSi5Cu1Mg DIN EN 1676: 2019
EN AC-45300 DIN EN 1706: 2013
EN AC-AlSi5Cu1Mg DIN EN 1706: 2013
EN AC-45300 DIN EN 1706: 2019
EN AC-AlSi5Cu1Mg DIN EN 1706: 2019
Domestic analogues
AK5MZch GOST 1583−93
AK5MVh GOST 1583−93
AL5−1 GOST 1583−93
AL5−1Z GOST 1583−93
AL5−1V GOST 1583−93
AL5−1 GOST 2685−75
AK5Mch GOST R 55375−12
Analogs in the USA
A305.0 AA
EN AC-45300 ASME SB / EN 1706
EN AC-AlSi5Cu1Mg ASME SB / EN 1706
For the manufacture of shaped castings. The alloy is made from recycled waste. The chemical composition of the alloy varies widely, therefore, its physicochemical properties are unstable. Aluminum AK5MCh is supplied in ingots, ingots, pyramids, granules. Technical requirements: GOST 1583−93 Cast aluminum alloys. Technical conditions GOST R 55375−12 Primary aluminum and alloys based on it. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |