Alloy aluminum AK9TS6 (AK9TS6r)
For the manufacture of ingots and shaped castings. Technical requirements — according to GOST 1583−93 Cast aluminum alloys. Technical conditions GOST R 55375−12 Primary aluminum and alloys based on it. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | 0.3–1 | 8–10 | 0.3–0.5 | 0.1–0.6 | 0.3–1.5 | 5–7 | < 0.3 | 79.1–86 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 1583-93 | in chill mold | 147–167 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Castings | GOST 1583-93 | 70–80 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |