Aluminum alloy AK9M2
For the manufacture of ingots and shaped castings by various casting methods (die casting, die casting) Technical requirements GOST R 55375−12 Primary aluminum and alloys based on it. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 1.2 | 7.5–10 | 0.2–0.8 | 0.1–0.4 | < 0.1 | 0.05–0.2 | 0.5–2 | < 1.2 | < 0.5 | 83.6–91.65 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 1583-93 | in chill mold | 186–274 |
Analogues
| USA |
|---|
| SG 100A |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |