Alloy aluminum AK9P
Chemical composition
| Al | Aluminum | Rest |
| Be | Beryllium | <0.0005 |
| Fe | Iron | <0.8 |
| Si | Silicon | 8.0 — 11.0 |
| Mg | Magnesium | 0.25 — 0.45 |
| Mn | Manganese | 0.2 — 0.5 |
| Cu | Copper | <1.0 |
| As | Arsenic | <0.015 |
| Ni | Nickel | <0.3 |
| Sn | Tin | <0.02 |
| Pb | Lead | <0.15 |
| Ti | Titanium | <0.2 |
| Zn | Zinc | <0.3 |
| Ot | Total impurities | <2.4 |
Casting methods:
Z — sand casting
B — Lost wax casting
K — chill casting
D — injection molding
Mark designation:
h — clean
bees — high purity
och — high purity
l — casting alloys
c — selective
For the manufacture of food products. Technical requirements — according to GOST 1583−93
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | As, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 1.3 | 8–11 | < 0.0005 | 0.2–0.4 | 0.2–0.5 | < 1 | < 0.3 | < 0.3 | 85.0345–91.6 | < 0.15 | < 0.015 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |