Alloy aluminum AL13 (AMg5K)
Chemical composition
| Al | Aluminum | Rest |
| Fe | Iron | <1.5 |
| Si | Silicon | 0.8 — 1.3 |
| Mg | Magnesium | 4.5 — 5.5 |
| Mn | Manganese | 0.1 — 0.4 |
| Cu | Copper | <0.1 |
| Zn | Zinc | <0.2 |
| Zr | Zirconium | <0.15 |
| Ot | Total impurities | <1.8 |
AlMg5 DIN 1725 Part 1
3.3555 DIN 1725 Part 1
GK-AlMg5 DIN 1725 Part 2
3.3561.02 DIN 1725 Part 2
G-AlMg5 DIN 1725 Part 2
3.3561.01 DIN 1725 Part 2
GB-AlMg5 DIN 1725 Part 5
3.3562 DIN 1725 Part 5
244 DIN 1725 Part 5
EN AC-51300 DIN EN 12392: 2016
EN AC-AlMg5 DIN EN 12392: 2016
EN AC-51300 DIN EN 12392: 2016 / A1: 2019
EN AC-AlMg5 DIN EN 12392: 2016 / A1: 2019
AW-5019 DIN EN 1301−2: 1997
EN AW-5019 DIN EN 1301−2: 1997
AlMg5 DIN EN 1301−2: 1997
EB AB-51300 DIN EN 1676: 2010
EN AB-AlMg5 DIN EN 1676: 2010
EN AC-51300 DIN EN 1706: 2013
EN AC-51400 DIN EN 1706: 2013
EN AC-AlMg5 DIN EN 1706: 2013
EN AC-AlMg5 (Si) DIN EN 1706: 2013
EN AC-51300 DIN EN 1706: 2019
EN AC-AlMg5 DIN EN 1706: 2019
EN AC-51400 DIN EN 1706: 2019
EN AC-AlMg5 (Si) DIN EN 1706: 2019
EN AW-5019 DIN EN 573−3: 2013
EN AW-AlMg5 DIN EN 573−3: 2013
Aluminum alloys DIN EN 601: 2004
Aluminum alloys DIN EN 602: 2004
AlMg5 TGL 14725
AlMg5 TGL 6556/02
AlMg5Si TGL 6556/02
244 VDS
245 VDS
Analogs in Russia
AMg5P Included in 3 standards
AMg5 Included in 4 standards
AMg5K GOST 1583−93
AL13 GOST 1583−93
AL28 GOST 1583−93
AL28Z GOST 1583−93
AL28V GOST 1583−93
AMg5M GOST 21631−76
AL13 GOST 2171−90
D45 GOST 2171−90
AL28 GOST 2685−75
1550 GOST 4784−97
1557 GOST 4784−97
AMg5K GOST R 55375−12
AL13 GOST R 55375−12
AMg5Mts GOST R 55375−12
AL28 GOST R 55375−12
1550 RS
Analogs in the USA
5056A
4177 AMS
4182 AMS
4349 AMS
AMS-A-81596 AMS
AA5019 ANSI
EN AC-51300 ASME SB / EN 1706
EN AC-51400 ASME SB / EN 1706
EN AC-AlMg5 ASME SB / EN 1706
EN AC-AlMg5 (Si) ASME SB / EN 1706
B 211 (5056) ASTM B211
B 26 (514.0) ASTM B26
B 26 (A05140) ASTM B26
B 275 (A 05140) ASTM B275
B 275 (A 95056) ASTM B275
B 316 (5056) ASTM B316
B 618 (514.0) ASTM B618
F 1667 (5056) ASTM F1667
J452 (320) SAE J452
A05140 UNS
A95056 UNS
514.0 Included in 2 standards
5056 Included in 7 standards
For the manufacture of shaped castings; the alloy is corrosion resistant. Technical requirements GOST 1583−93 Cast aluminum alloys. Technical conditions GOST 2171−90 Parts, products, semi-finished products and billets of non-ferrous metals and alloys. Designation of the brand GOST 2685−75 Cast aluminum alloys. GOST R 55375−12 grades Primary aluminum and alloys based on it. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Zr, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 1.5 | 0.8–1.3 | 4.5–5.5 | 0.1–0.4 | < 0.1 | < 0.2 | < 0.15 | 91–94.6 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
|---|---|
| 20 | 20 |
Mechanical properties at 20 °C
Casting and technological parameters
| linear shrinkage, % |
|---|
| 1.2 |
Analogues
| USA | Germany |
|---|---|
| 512 | G-AlMg5 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter | Units of measurement | Description |
|---|---|---|
| linear shrinkage | % | The difference between model dimensions and the model casting |