Aluminum alloy AL23-1 (AMg6lch)
Chemical composition
| Al | Aluminum | Rest |
| Be | Beryllium | 0.02 — 0.10 |
| Fe | Iron | <0.05 |
| Si | Silicon | <0.05 |
| Mg | Magnesium | 6.0 — 7.0 |
| Mn | Manganese | <0.1 |
| Cu | Copper | <0.05 |
| Ti | Titanium | 0.05 — 0.15 |
| Zn | Zinc | <0.05 |
| Zr | Zirconium | 0.05 — 0.20 |
| Ot | Total impurities | <0.2 |
AMg6 Included in 4 standards
AMg6l GOST 1583−93
AL23 GOST 1583−93
AMg6lch GOST 1583−93
AL23−1 GOST 1583−93
AMg6B GOST 17232−99
AMg6M GOST 21631−76
AMg6BM GOST 21631−76
AMg6B GOST 21631−76
AMg6UM GOST 21631−76
AMg6U GOST 21631−76
D46 GOST 2171−90
AL23 GOST 2685−75
1560 GOST 4784−97
AMg6l GOST R 55375−12
AL23 GOST R 55375−12
AMg6lch GOST R 55375−12
AL23−1 GOST R 55375−12
Analogs in the USA
220
Almag 35
Almag 535
535.0 ANSI
SB 108 (A05350) ASME SB108
SB 108 (535.0) ASME SB108
B 108 (535.0) ASTM B108
B 108 (A05350) ASTM B108
B 26 (520.0) ASTM B26
B 26 (A05200) ASTM B26
B 26 (535.0) ASTM B26
B 26 (A05350) ASTM B26
B 275 (A 05200) ASTM B275
B 275 (A 05 350) ASTM B275
B 618 (520.0) ASTM B618
B 618 (535.0) ASTM B618
J452 SAE J452
J452 SAE J452
A05200 UNS
A05350 UNS
520 Included in 2 standards
520.0 Included in 2 standards
535.0 Included in 2 standards
For the manufacture of parts with increased corrosion resistance. Technical requirements GOST 1583−93 Cast aluminum alloys. Technical conditions GOST 2685−75 Cast aluminum alloys. GOST R 55375−12 grades Primary aluminum and alloys based on it. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.05 | < 0.05 | 0.02–0.1 | 6–7 | < 0.1 | 0.05–0.15 | < 0.05 | < 0.05 | 0.05–0.2 | 92.35–93.88 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Analogues
| USA |
|---|
| 535 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |