AL32Z
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Zr, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.7 | 7.5–9 | < 0.02 | 0.3–0.5 | 0.3–0.5 | 0.1–0.3 | 1–1.5 | < 0.3 | < 0.02 | < 0.1 | 86.14–90.8 | < 0.02 | < 0.9 |
Note: Casting methods: Z - sand casting; B - lost-wax casting; K - chill casting; D - injection molding
Note: Designation of grades: h - pure bees - high purity och - high purity l - casting alloys with - selective
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| АЛ32З | 328 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Pb | % | Lead |