AMg4K1.5M (AMg4K1.5M1)
For the manufacture of ingots and shaped castings.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.4 | 1.3–1.7 | 0.002–0.004 | 4.5–5.2 | 0.6–0.9 | 0.1–0.25 | 0.7–1 | < 0.1 | 90.446–92.798 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 1583-93 | in chill mold | 211–265 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Casting | GOST 1583-93 | 81–104 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |