AMg5 (1550)
For the manufacture of semifinished products by hot or cold deformation
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Be, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
| GOST 4784-97 |
< 0.5 |
< 0.5 |
0.0002–0.005 |
4.8–5.8 |
0.3–0.8 |
0.02–0.1 |
< 0.1 |
< 0.2 |
91.9–94.68 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
71 |
|
2650 |
|
0.064 |
| 100 |
|
126 |
|
0.922 |
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Trumpet |
|
|
|
|
255 |
110 |
15 |
|
| Round |
GOST 21488-97 |
|
|
|
245–265 |
110–120 |
10–15 |
|
| Tape |
|
|
|
|
275 |
130 |
12–15 |
|
| Profile |
|
|
|
|
255 |
127 |
15 |
|
| Sheet |
|
|
|
|
255–265 |
110–120 |
12–13 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
|
65 |
Analogues
| Germany |
USA |
| 3.3555 |
AA5056 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Be |
% |
Beryllium |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$c\cdot 10^{-3}$$ |
$$\frac{J}{kg\cdot K}$$ |
The specific heat of the material (range 20°C–T) |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |