Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zr, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.5 | < 0.3 | 4.8–6.3 | 0.4–1 | 0.05–0.15 | < 0.3 | < 0.1 | 91.35–94.75 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|
| Castings | GOST 1583-93 | 196–206 | 3.5–5 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Alloy | GOST 1583-93 | 55 |
Analogues
| Germany | USA |
|---|---|
| EN AW-5456 | 5456A |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 | |
| GOST Р 55375-2012 | |
| DSTU 2839-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zr | % | Zirconium |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |