AMg7 (AL29)
for the production of shaped castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.9 | 0.5–1 | < 0.01 | 6–8 | 0.25–0.6 | < 0.1 | < 0.2 | 89.19–93.25 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|
| Castings | GOST 1583-93 | 206 | 3 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| injection molding | GOST 1583-93 | 60 |
Analogues
| USA |
|---|
| A535.0 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 | |
| GOST Р 55375-2012 | |
| DSTU 2839-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |