BrAZhNMts9-4-4-1
Pipe boards capacitors, parts of chemical equipment; semi-finished products (bars, forgings)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Pressureless bronze plated |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | P, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 18175-78 | 4–5 | < 0.1 | < 0.1 | 0.5–1.2 | 78.1–82.7 | < 0.5 | 4–5 | 8.8–10 | < 0.02 | < 0.01 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Analogues
| USA | Germany |
|---|---|
| C63200 | CuAl10Fe4Ni5 |
Standards
| Standard | Description |
|---|---|
| GOST 18175-78 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
| P | % | Phosphorus |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |