BrAMts10-2
Billets, mold casting in the shipbuilding industry;
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Pressureless bronze plated |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Al, % | Pb, % | P, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 18175-78 | < 0.5 | < 0.1 | < 0.1 | 1.5–2.5 | 84.8–89.5 | < 1 | 9–11 | < 0.03 | < 0.01 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Analogues
| Germany | USA |
|---|---|
| AlBz9Mn | ERCuAl-A2 |
Standards
| Standard | Description |
|---|---|
| GOST 18175-78 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |
| P | % | Phosphorus |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |