BrB2.5
for the manufacture of springs and elastic members;
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Pressureless bronze plated |
Chemical composition
| Standard |
Fe, % |
Si, % |
Be, % |
Cu, % |
Ni, % |
Al, % |
Pb, % |
| TU 48-21-96-72 |
< 0.15 |
< 0.15 |
2.3–2.6 |
96.4–97.5 |
0.2–0.5 |
< 0.15 |
< 0.005 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
133 |
16.6 |
8230 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Alloy |
|
|
|
soft |
580 |
25 |
|
| Alloy |
|
|
|
solid |
1350 |
1–2 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
soft |
130 |
| Alloy |
|
solid |
360 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Be |
% |
Beryllium |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |