BrBNT1.9Mg
Springs, springy parts-duty, wear-resistant parts of all kinds, non-sparking tools
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Pressureless bronze plated |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Ti, % | Cu, % | Ni, % | Al, % | Pb, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 18175-78 | < 0.15 | < 0.15 | 1.85–2.1 | 0.07–0.13 | 0.1–0.25 | 96.62–97.78 | 0.2–0.4 | < 0.15 | < 0.005 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$E\cdot 10^{9}$$, $$MPa$$ |
|---|---|
| 20 | 125 |
Standards
| Standard | Description |
|---|---|
| GOST 18175-78 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$E\cdot 10^{9}$$ | $$MPa$$ | Elastic modulus |