Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
Cp, Дж/кг·К |
| 20 |
1.04 |
48.1 |
8800 |
368.4 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
δ, % |
Treatment |
| Chill casting |
GOST 1583-93 |
|
|
|
295 |
|
3–10 |
|
| Sand casting |
GOST 1583-93 |
|
|
|
215 |
175 |
3–10 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Casting |
GOST 613-79 |
in chill mold |
108 |
| Casting |
GOST 613-79 |
in sandy form |
68–78 |
Casting and technological parameters
Coefficients of Friction
| coefficient of friction with lubrication |
coefficient of friction without lubrication |
| 0.0056 |
0.17 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| Cp |
Дж/кг·К |
Specific heat of material |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| δ |
% |
Elongation after rupture |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |