BrSr0.1
Switches, collector ring, rotor turbine generators winding
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Pressureless bronze plated |
Chemical composition
| Standard |
Cu, % |
Ag, % |
O, % |
| GOST 18175-78 |
99.72–99.82 |
0.08–0.12 |
< 0.06 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
127 |
17 |
8890 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Alloy |
|
|
|
soft |
200 |
80 |
55 |
|
| Alloy |
|
|
|
solid |
340 |
300 |
4 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
soft |
50 |
| Alloy |
|
solid |
110 |
Casting and technological parameters
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Cu |
% |
Copper |
| Ag |
% |
Silver |
| O |
% |
Oxygen |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |