CHH22
for the details with high resistance to abrasion and wear in a milling equipment, screens and slide-ways, and pesko- sintering machines and shot blasting chambers at elevated temperatures.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | High alloy cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 7769-82 | 67.02–76.6 | 0.2–1 | 1.5–2.5 | 19–25 | 0.15–0.35 | 0.15–0.35 | < 0.1 | 2.4–3.6 | < 0.08 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 7769-82 | 290 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 7769-82 | 330–610 |
Standards
| Standard | Description |
|---|---|
| GOST 7769-82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |