CHS15
for parts with high corrosion resistance to concentrated acids, alkalis, salt solutions (except hydrofluoric and fluorine compounds) at temperatures up to 200 degrees C; Avoid abrupt variables, as well as shock and temperature changes.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | High alloy cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| GOST 7769-82 | 82.23–85.6 | 14.1–16 | < 0.8 | < 0.1 | 0.3–0.8 | < 0.07 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 7769-82 | 60 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 7769-82 | 290–390 |
Standards
| Standard | Description |
|---|---|
| GOST 7769-82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |