CHS5SH
for parts with heat resistance of the flue gases and the air to 800 degrees C
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Low alloy cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| GOST 7769-82 | 89.77–92.7 | 4.5–5.5 | < 0.8 | < 0.2 | 0.1–0.3 | < 0.1 | 2.7–3.3 | < 0.03 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 7769-82 | 290 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 7769-82 | 228–300 |
Standards
| Standard | Description |
|---|---|
| GOST 7769-82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |