CHYU22SH
for parts with heat resistance in air up to 1100 degrees C; heat resistant in environments containing sulfur, sulfur dioxide, vanadium oxides, water vapor; high strength at normal and elevated temperatures.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | High alloy cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| GOST 7769-82 | 69.47–78.4 | 1–2 | < 0.8 | 19–25 | < 0.2 | 1.6–2.5 | < 0.03 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Casting | GOST 7769-82 | 290 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 7769-82 | 241–364 |
Standards
| Standard | Description |
|---|---|
| GOST 7769-82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |