Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
W, % |
| GOST 5632-72 |
60.58–67.7 |
< 0.45 |
8–10 |
20–22 |
< 0.2 |
< 0.3 |
3.5–4.5 |
< 0.2 |
< 0.04 |
0.5–0.6 |
< 0.03 |
< 0.3 |
0.3–0.6 |
< 0.2 |
Information on suppliers
Properties
| Property |
| Calculated Properties Density: 7.66 g / cm3 |
Analogues
| Germany |
USA |
| 1.4871 |
K63008 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| W |
% |
Tungsten |